Talking about the stone carving antique old steps

With the improvement of living standards, modern people's thinking has begun to change, the antique style has become more and more intense, and the art of stone carving has become more and more popular. In this way, antique stone carvings are becoming more and more popular. In people's concepts and understanding, antique stone carvings are generally treated in the same way as fake ancient stone carvings. In fact, imitation and pseudo are two different concepts. Imitation is imitation and emulation, while fake ancient stone carving is different, pseudo is fake, that is, pure fake.

(1) Brush the surface of the stone with nitric acid or hydrochloric acid. The stone surface has been corroded due to chemical reactions. It can be placed in the open air in the summer, and it is similar to the cultural relics. It is black and bright due to the water of nitric acid or hydrochloric acid. Moreover, it has a wrinkled skin on the top 4). But there are no such things in real artifacts.

(2) The stone carvings are fired with fire, and the yellow soil is used to smear the loess, and the soil is shaped after being dried.

(3) The stone carvings are cooked for a few days with a large amount of smoked water. The stone carving is taken out and dried to give a color like iron rust.

(4) The effect of boiling stone carving with Tenghuangbaiyu for several days, the same effect as (3).

(5) Using a fragrant head to smoke a layer of original tires, place them in the sunny place, spray water several times a day, and then, after several months, brush the floating ash floating soil with cool water, and the remaining glaze and stone carvings Real loess rust is almost the same.

(6) Wash with potassium permanganate and apply it to the stone statue. After infiltrating the potassium permanganate into the inside, according to the requirements of the color depth, rinse the surface with clean water, then wipe with a little yellow mud. Once again, you can achieve the effect of antique works. Here you need to know the real stone carving artifacts. If you use alkaline water, the rust will not peel off. If the rust is fake, it is realistic, but its rust is no longer present with alkaline water.

(7) Using an oxygen gun for fire treatment, according to the hardness of different stones, the time of the fire is 4-9 seconds, the distance of the oxygen gun from the surface of the stone is controlled at 6-11 cm, and the burnt area of ​​the stone is 75- 96, then use the iron brush to clean the hair, depending on the old and old degree, use the brown hair machine to polish through, then apply the Chen tea juice 47, add ink 3.1, rust juice 4.3, after drying and waxing, to reach the stone antique requirements.  

The preparation technology of Si3N4 ceramics has developed rapidly in the past few years. The preparation process mainly concentrates on reaction sintering method, hot pressing sintering method, atmospheric pressure sintering method, gas pressure sintering method, etc. Due to different preparation processes, various types of Silicon Nitride Ceramics have Different microstructures (such as porosity and pore morphology, grain morphology, intergranular morphology, and intercrystalline second phase content). Therefore, the performance varies greatly. In order to obtain Si3N4 ceramic materials with excellent performance, high-quality Si3N4 powder should be prepared first. The quality of Si3N4 powder prepared by different methods is not exactly the same, which leads to the difference in its application. The failure of many ceramic materials is often attributed to Developers do not understand the differences between various ceramic powders and have insufficient knowledge of their properties.

Silicon Nitride Ceramic Shaft

Silicon Nitride Ceramic Shaft,Black Silicon Nitride Ceramic Shaft,Machinable Glass Ceramic Shaft,Customized Machining Silicon Nitride Ceramic

SHENZHEN HARD PRECISION CERAMIC CO.,LTD , http://www.hardcm.com